BaTiO3 200/300/400/500nm 99.9% Tetragonal
- Send E-mail to us:sales1@rboschco.com
- Tel:+86 (0379)65110019
- Fax:+86 (0379) 65110031
We're here to help Easy ways to get the answers you need.
Moisture (at 105oC, 2h): 0.11wt%
Ignition Loss (at 1100oC, 1h): 0.27wt%
Barium Titanate Nanopowder (BaTiO3,Tetragonal) Certificate of Analysis-wt%
|
|||||
Na |
Ca |
Fe |
K |
Mg |
Sr |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.018 |
Ba/Ti |
1.000 |
Ignition Loss (at 1100oC, 1h): 0.27wt%
Barium Titanate Nanopowder (BaTiO3,Tetragonal) Certificate of Analysis-wt%
|
|||||
Na |
Ca |
Fe |
K |
Mg |
Sr |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.019 |
Ba/Ti |
1.000 |
Ignition Loss (at 1100oC, 1h): 0.20wt%
Barium Titanate Nanopowder (BaTiO3,Tetragonal) Certificate of Analysis-wt%
|
|||||
Na |
Ca |
Fe |
K |
Mg |
Sr |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.020 |
Ba/Ti |
1.000 |
Barium Titanate Nanopowder (BaTiO3,Tetragonal) 500nm
Moisture (at 105oC, 2h): 0.09wt%
Ignition Loss (at 1100oC, 1h): 0.13wt%
Making method: Preparation of Electronic Nanomaterials by Combustion Method
Barium Titanate Nanopowder (BaTiO3,Tetragonal) Certificate of Analysis-wt%
|
|||||
Na |
Ca |
Fe |
K |
Mg |
Sr |
0.001 |
0.001 |
0.001 |
0.001 |
0.001 |
0.019 |
Ba/Ti |
1.000 |
Applications for Barium Titanate Nanopowder (BaTiO3,Tetragonal):
High-density optical data storage; Phase conjugated mirrors and lasers; Nonlinear optical devices; Pattern recognition; Micro-capacitors; Ferroelectric ceramics; PTC thermistors; On-chip programmable devices; Optical computing; Optical image processing; Piezoelectric devices; Pyroelectric sensors; Semiconductive ceramics; Varistors; Electro-optic devices; Ceramic capacitors; Dielectric amplifiers; Dynamic holography.